我厂新(xīn)工艺線(xiàn)的熟料率值设计控制指标為(wèi)多(duō)少?

普通水泥熟料: 
KH=0.900.02 
SM=2.60.1 
AM=1.60.1 
特种水泥熟料: 
KH=0.860.01 
SM=2.60.1 
AM=1.00.1 
C3S=501.0%, C3A=4.00.5%, Na2O.Eq≤0.55% 
低碱水泥熟料: 
KH=0.880.01 
SM=2.60.1 
AM=1.60.1 
Na2O.Eq≤0.55%
 
 
 